Type 430 Stainless Steel Wire
ASTM A580
Stainless steel grade 430 is a non-hardenable steel containing straight chromium, and belongs to the ferritic group of steels. This steel is known for its good corrosion resistance and formability, coupled with practical mechanical properties. It can be used in certain chemical applications due to its resistance to nitric acid. This product is often used for fasteners as well as lashing wire.
Can be supplied in bright and soap coated finish.
Chemical Requirements (Composition, %)
Stainless Steel Authentic Grades
UNS# | Type | C, Max | mn, max | p, max | s, max | si, max | cr | ni | mo | n |
---|---|---|---|---|---|---|---|---|---|---|
S30200 | 302 | 0.15 | 2.00 | 0.045 | 0.030 | 1.00 | 17.0-19.0 | 8.0-10.0 | 0.10max | |
S30215 | 302B | 0.15 | 2.00 | 0.045 | 0.030 | 2.00-3.00 | 17.0-19.0 | 8.0-10.0 | ||
S30400 | 304 | 0.08 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0-20.0 | 8.0-10.5 | 0.10max | |
S30403 | 304L | 0.030 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0-20.0 | 8.0-12.0 | 0.10max | |
S31600 | 316 | 0.08 | 2.00 | 0.045 | 0.030 | 1.00 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | 0.10max |
S31603 | 316L | 0.030 | 2.00 | 0.045 | 0.030 | 1.00 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | 0.10max |
Stainless Steel Ferritic Grades
UNS# | Type | C, Max | mn, max | p, max | s, max | si, max | cr | ni | mo | n |
---|---|---|---|---|---|---|---|---|---|---|
S43000 | 430 | 0.12 | 1.00 | 0.040 | 0.030 | 1.00 | 16.0-18.0 | 0.10max |
Mechanical Test Requirements
Austenitic Grades
UNS# | type | condition | final operation |
tensile strength
min. (ksi) |
yield strength
min. (ksi) |
Elongation in Length 4x Gage Diameter of
Test Specimens, min, % |
Reduction of Area, min, % |
---|---|---|---|---|---|---|---|
S30200
S30215 S30400 S31600 |
302
302B 304 316 |
A | Cold Finished | 90 | 45 | 30 | 40 |
S30200
S30215 S30400 S31600 |
302
302B 304 316 |
A | Annealed | 75 | 30 | 35 | 50 |
S30403
S31603 |
304L
316L |
A | Cold Finished | 90 | 45 | 30 | 40 |
S30403
S31603 |
04L
316L |
A | Annealed | 70 | 25 | 35 | 50 |
Ferritic Grades
UNS# | type | condition | final operation |
tensile strength
min. (ksi) |
yield strength
min. (ksi) |
Elongation in Length 4x Gage Diameter of
Test Specimens, min, % |
Reduction of Area, min, % |
---|---|---|---|---|---|---|---|
43000 | 430 | A | Cold Finished | 70 | 40 | 16 | 45 |
43000 | 430 | A | Annealed | 70 | 40 | 20 | 45 |
Minimum unless otherwise noted.